Romania STAS/SR RU12v tool steel and RU12v Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Tool Steel And Hard Alloy | RU12v | STAS/SR | Romania | tool steel | 
| Rp2 | |||||
| Rp3 | |||||
| Rp4 | |||||
| Rp5 | |||||
| Rp9 | |||||
| Rp10 | |||||
| Rp11 | |||||
| RUL1 | |||||
| RU12 | |||||
| RU11v | 
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) | Cu(%) | 
|---|---|---|---|---|---|---|---|---|
| 0.95 -1.10 | 0.40-0.65 | 0.90-1.20 | 0.027 | 0.02 | 1.30-1. 65 | 0.30 | 0.08 | 0.25 | 
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 464 (≥) | 627 (≥) | 11 | 41 | 44 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 134 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 11 | - | - | 0.22 | - | |||
| 252 | 792 | - | 23.3 | 223 | - | ||
| 856 | - | 22 | 21.2 | 433 | 143 | 
Heat treated : 1649°C - 1138°C