Euronorm EN EN X210Cr12 Euronorm Tool steel and EN X210Cr12 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Tool Steel And Hard Alloy | EN X210Cr12 | EN | Euronorm | Euronorm Tool steel | 
| EN 60WCrV8 | |||||
| EN 70MnMoCr8 | |||||
| EN 90MnCrV8 | |||||
| EN 95 MnWCrS | |||||
| EN 102Cr6 | |||||
| EN 105V | |||||
| EN X38CrMo16 | |||||
| EN X40Cr11 | |||||
| EN X100CrMoV5 | |||||
| EN X153CrMoV12 | 
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 945 (≥) | 783 (≥) | 22 | 41 | 44 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 111 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 21 | - | - | 0.13 | - | |||
| 378 | 755 | - | 32.3 | 442 | - | ||
| 127 | - | 11 | 23.2 | 132 | 124 | 
Heat treated : 1738°C - 1315°C
| Grade | Standard | Country | Application | 
|---|---|---|---|
| X210Cr12 | DIN | Germany | Cold working alloy tool steel | 
| 35CrMo7 | ISO | ISO | Carbide for cutting tools | 
| 35CrMo7 | ISO | ISO | Carbide for cutting tools | 
| X210Cr12 | UNE | Spain | Spain structural alloy steel | 
| EN X210Cr12 | EN | Euronorm | Euronorm Tool steel | 