Euronorm EN EN HS3-3-2 Euronorm Tool steel and EN HS3-3-2 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Tool Steel And Hard Alloy | EN HS3-3-2 | EN | Euronorm | Euronorm Tool steel | 
| EN X30WCrV9-3 | |||||
| EN X35CrWMoV5 | |||||
| EN X37CrMoV5-1 | |||||
| EN X38CrMoV5-3 | |||||
| EN X40CrMoV5-1 | |||||
| EN HS1-4-1 | |||||
| EN HS1-4-2 | |||||
| EN HS1-8-1 | |||||
| EN HS2-9-1-8 | |||||
| EN HS2-9-2 | 
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 968 (≥) | 243 (≥) | 33 | 32 | 41 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 443 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 14 | - | - | 0.34 | - | |||
| 675 | 788 | - | 23.3 | 143 | - | ||
| 612 | - | 13 | 43.2 | 331 | 331 | 
Heat treated : 1658°C - 1185°C
| Grade | Standard | Country | Application | 
|---|---|---|---|
| HS3-3-2 | ISO | ISO | Carbide for cutting tools | 
| HS3-3-2 | ISO | ISO | Carbide for cutting tools | 
| EN HS3-3-2 | EN | Euronorm | Euronorm Tool steel | 
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com