Germany DIN 1.2762 Cold working alloy tool steel and 1.2762 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Tool Steel And Hard Alloy | 1.2762 | DIN | Germany | Cold working alloy tool steel | 
| 1.2735 | |||||
| 15NiCr14 | |||||
| 40CrMnNiMo8-6-4 | |||||
| 1.2738 | |||||
| 1.2743 | |||||
| 60NiCrMoV12-4 | |||||
| 1.2745 | |||||
| 15NiCr18 | |||||
| 1.2746 | |||||
| 45NiCrMoV16-6 | 
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) | W(%) | 
|---|---|---|---|---|---|---|---|---|
| 0.70-0.80 | 0.15-0.30 | 0.15-0.53 | Max 0.035 | Max 0.035 | 1.40-1.60 | 0.40-0.60 | 0.60-0.80 | 0.20-0.40 | 
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 285 (≥) | 477 (≥) | 24 | 44 | 12 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 314 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 32 | - | - | 0.43 | - | |||
| 856 | 311 | - | 11.3 | 311 | - | ||
| 928 | - | 32 | 12.2 | 133 | 314 | 
Heat treated : 1333°C - 1973°C