Romania STAS/SR 14CrMo4 Structural steel and 14CrMo4 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Structure Steel | 14CrMo4 | STAS/SR | Romania | Structural steel | 
| 35Mn14 | |||||
| 35VMoMn14 | |||||
| 40VMoMnCr7 | |||||
| 41MoCr11 | |||||
| 43MoMn16 | |||||
| OLT35 | |||||
| OI.T45 | |||||
| OLT65 | |||||
| 10CrMOL0 | |||||
| 10MoCr50 | 
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) | Cu(%) | Ti(%) | 
|---|---|---|---|---|---|---|---|---|---|
| 0.10-0.18 | 0.15-0.35 | 0.40 -0.70 | 0.040 | 0.040 | 0.70-1.00 | 0.30 | 0.40-0.55 | 0.30 | 0.02 | 
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 398 (≥) | 185 (≥) | 44 | 13 | 41 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 241 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 12 | - | - | 0.21 | - | |||
| 351 | 176 | - | 43.3 | 341 | - | ||
| 855 | - | 32 | 31.2 | 311 | 143 | 
Heat treated : 1452°C - 1328°C
| Grade | Standard | Country | Application | 
|---|---|---|---|
| 14CrMo4 | STAS/SR | Romania | Structural steel | 
| 14CrMo4 | STAS/SR | Romania | Structural steel | 
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com