X6CrNiMo17-12-2 Stainless Steel and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Stainless Steel | X6CrNiMo17-12-2 | |||
| X1CrNiMoCu25-20-5 | |||||
| X6CrNiTi18-10 | |||||
| X5NiCrCuNb16-4 | |||||
| X6CrNiNb18-10 | |||||
| X2CrNiAlTi32-20 | |||||
| X1CrNiMoCu32-28-7 | |||||
| X1NiCrMoCuN31-27-4 | |||||
| X2CrNiMnMoNbN 25-18-5-4 | |||||
| X3CrNiCu 18-9-4 | |||||
| X7CrNiAl 17-7 | 
| C | Si ≤ | Mn ≤ | P ≤ | S ≤ | Cr | Ni | Mo | Other | 
|---|---|---|---|---|---|---|---|---|
| ≤0.08 | 1.00 | 2.00 | 0.045 | 0.015 | 16.5-18.5 | 10.5-13.5 | 2.00-2.50 | Ti ≥5*C≤0.70 | 
	 
	.
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 363 (≥) | 874 (≥) | 31 | 12 | 24 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 244 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 13 | - | - | 0.42 | - | |||
| 935 | 576 | - | 24.3 | 334 | - | ||
| 597 | - | 12 | 24.2 | 313 | 441 | 
Heat treated : 1154°C - 1812°C
| Grade | Standard | Country | Application | 
|---|---|---|---|
| X6CrNiMo17-12-2 | DIN | Germany | Stainless steel | 
| EN X6CrNiMo17-12-2 | EN | Euronorm Stainless Steel | 
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com