X2CrNiN18-7 Stainless Steel and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Stainless Steel | X2CrNiN18-7 | |||
| X20CrMo13 | |||||
| X39CrMo17-1 | |||||
| X105CrMo17 | |||||
| X5CrNi18-10 | |||||
| X4CrNi18-12 | |||||
| X8CrNiS18-9 | |||||
| X2CrNi19-11 | |||||
| X10CrNi18-8 | |||||
| X2CrNiN18-10 | |||||
| X3CrNi13-4 | 
| C | Si ≤ | Mn ≤ | P ≤ | S ≤ | Cr | Ni | Mo | Other | 
|---|---|---|---|---|---|---|---|---|
| ≤0.030 | 1.00 | 2.00 | 0.045 | 0.015 | 16.5-18.5 | 6.00-8.00 | -------- | N 0.10-0.20 | 
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 361 (≥) | 377 (≥) | 34 | 31 | 13 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 114 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 21 | - | - | 0.43 | - | |||
| 674 | 924 | - | 12.3 | 144 | - | ||
| 886 | - | 22 | 24.2 | 133 | 132 | 
Heat treated : 1327°C - 1884°C
| Grade | Standard | Country | Application | 
|---|---|---|---|
| X2CrNiN18-7 | AFNOR | France | Austenite | 
| ISO X2CrNiN18-7 | ISO standard thermal deformation of stainless steel | ||
| EN X2CrNiN18-7 | EN | Euronorm Stainless Steel | |
| EN X2CrNiN18-7 | EN | Euronorm Stainless Steel | 
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com