X14CrMoS17 Stainless Steel and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Stainless Steel | X14CrMoS17 | |||
| X12CrS13 | |||||
| X12Cr13 | |||||
| X6Cr17 | |||||
| X20Cr13 | |||||
| X15Cr13 | |||||
| X30Cr13 | |||||
| X39Cr13 | |||||
| X46Cr13 | |||||
| X65Cr13 | |||||
| X17CrNi16-2 | 
| C | Si ≤ | Mn ≤ | P ≤ | S ≤ | Cr | Ni | Mo | Other | 
|---|---|---|---|---|---|---|---|---|
| 0.10-0.17 | 1.00 | 1.50 | 0.040 | 0.15-0.35 | 15.5-17.5 | 0.20-0.60 | 
	 
	.
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 193 (≥) | 966 (≥) | 42 | 22 | 41 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 333 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 22 | - | - | 0.23 | - | |||
| 563 | 872 | - | 22.3 | 224 | - | ||
| 761 | - | 14 | 24.2 | 441 | 213 | 
Heat treated : 1447°C - 1441°C
| Grade | Standard | Country | Application | 
|---|---|---|---|
| ISO X14CrMoS17 | ISO standard thermal deformation of stainless steel | ||
| EN X14CrMoS17 | EN | Euronorm Stainless Steel | |
| EN X14CrMoS17 | EN | Euronorm Stainless Steel | 
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com