SUS444TB Stainless Steel and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Stainless Steel | SUS444TB | |||
| SUS329J4LTB | |||||
| SUS405TB | |||||
| SUS409TB | |||||
| SUS409LTB | |||||
| SUS410TB | |||||
| SUS410TiTB | |||||
| SUS430TB | |||||
| SUS430LXTB | |||||
| SUS430J1LTB | |||||
| SUS436LTB | 
| C ≤ | Si ≤ | Mn ≤ | P ≤ | S ≤ | Cr | Ni | 
|---|---|---|---|---|---|---|
| 0.025 | 1.0 | 1.0 | 0.04 | 0.03 | 17-20 | ≤0.6 | 
| Mo | Al | Cu | Nb | Ti | V | Ce | 
| 1.75-2.5 | ||||||
| N | Co | Pb | B | Other Sum | ||
| ≤0.025 | 8*(C+N)~0.8 | |||||
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 928 (≥) | 328 (≥) | 12 | 41 | 34 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 111 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 22 | - | - | 0.32 | - | |||
| 553 | 777 | - | 21.3 | 231 | - | ||
| 353 | - | 21 | 44.2 | 411 | 122 | 
Heat treated : 1633°C - 1161°C
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...