SUS329J3L Stainless Steel and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Stainless Steel | SUS329J3L | |||
| SUS317L | |||||
| SUS317LN | |||||
| SUS317J1 | |||||
| SUS836L | |||||
| SUS890L | |||||
| SUS321 | |||||
| SUS347 | |||||
| SUSXM7 | |||||
| SUSXM15J1 | |||||
| SUS329J1 | 
| C ≤ | Si ≤ | Mn ≤ | P ≤ | S ≤ | Cr | Ni | 
|---|---|---|---|---|---|---|
| 0.03 | 1.0 | 2.0 | 0.04 | 0.03 | 21-24 | 4.5-6.5 | 
| Mo | Al | Cu | Nb | Ti | V | Ce | 
| 2.5-3.5 | ||||||
| N | Co | Pb | B | Other | ||
| 0.08-0.2 | ||||||
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 231 (≥) | 381 (≥) | 44 | 14 | 12 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 433 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 34 | - | - | 0.12 | - | |||
| 627 | 835 | - | 44.3 | 212 | - | ||
| 496 | - | 11 | 21.2 | 342 | 334 | 
Heat treated : 1397°C - 1335°C
| Grade | Standard | Country | Application | 
|---|---|---|---|
| SUS329J3L | JIS | Japan | Austenitic-ferritic (Duplex) stainless steels | 
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...