SUS321HTB Stainless Steel and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Stainless Steel | SUS321HTB | |||
| SUS310TB | |||||
| SUS310STB | |||||
| SUS312LTB | |||||
| SUS316TB | |||||
| SUS316HTB | |||||
| SUS316LTB | |||||
| SUS316TiTB | |||||
| SUS317TB | |||||
| SUS317LTB | |||||
| SUS321TB | 
| C ≤ | Si ≤ | Mn ≤ | P ≤ | S ≤ | Cr | Ni | 
|---|---|---|---|---|---|---|
| 0.04-0.1 | 0.75 | 2.0 | 0.03 | 0.03 | 17-20 | 9-13 | 
| Mo | Al | Cu | Nb | Ti | V | Ce | 
| 4*C~0.6 | ||||||
| N | Co | Pb | B | Other | ||
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 654 (≥) | 194 (≥) | 34 | 41 | 43 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 243 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 12 | - | - | 0.33 | - | |||
| 311 | 247 | - | 13.3 | 321 | - | ||
| 454 | - | 34 | 23.2 | 444 | 232 | 
Heat treated : 1898°C - 1922°C
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com