SUS316LN Stainless Steel and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Stainless Steel | SUS316LN | |||
| SUS304N2 | |||||
| SUS304LN | |||||
| SUS304J3 | |||||
| SUS305 | |||||
| SUS309S | |||||
| SUS310S | |||||
| SUS312S | |||||
| SUS316 | |||||
| SUS316L | |||||
| SUS316N | 
| C ≤ | Si ≤ | Mn ≤ | P ≤ | S ≤ | Cr | Ni | 
|---|---|---|---|---|---|---|
| 0.03 | 1.0 | 2.0 | 0.045 | 0.03 | 16.5--18.5 | 10.5-14.5 | 
| Mo | Al | Cu | Nb | Ti | V | Ce | 
| 2-3 | ||||||
| N | Co | Pb | B | Other | ||
| 0.1-0.22 | ||||||
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 799 (≥) | 335 (≥) | 22 | 33 | 33 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 433 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 14 | - | - | 0.31 | - | |||
| 962 | 628 | - | 21.3 | 314 | - | ||
| 577 | - | 21 | 12.2 | 333 | 322 | 
Heat treated : 1154°C - 1298°C