1.4704 Stainless Steel and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application |
|---|---|---|---|---|---|
| Steel Grades | Stainless Steel | 1.4704 | |||
| X53CrMnNiN 21-9 |
|||||
| X45CrNiW 18-9 |
|||||
| X55CrMnNiN 20-8 |
|||||
| X70CrMnNiN 21-6 |
|||||
| X50CrMnNiNbN 21-9 |
|||||
| NiFe25Cr20NbTi |
|||||
| 65Si7 |
|||||
| 37MnSi5 |
|||||
| 1.2731 |
|||||
| 1.3817 |
| C |
Si ≤ |
Mn ≤ |
P ≤ |
S ≤ |
Cr | Ni | Mo | Other |
|---|---|---|---|---|---|---|---|---|
| 0.40-0.50 | 3.50-4.50 | 1.00 | 0.045 | 0.030 | 2.50-3.00 | -------- | -------- | ------------ |
.
| Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
|---|---|---|---|---|---|---|
| 988 (≥) | 425 (≥) | 41 | 33 | 42 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 141 |
| Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
|---|---|---|---|---|---|---|---|
| 33 | - | - | 0.14 | - | |||
| 438 | 463 | - | 13.3 | 143 | - | ||
| 442 | - | 32 | 44.2 | 243 | 241 |
Heat treated : 1255°C - 1259°C
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com