France AFNOR Z8CDF19-02 Hot-Rolled stainless steel bar and wire rod (NF A 35-574 (1990)) and Z8CDF19-02 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application |
|---|---|---|---|---|---|
| Steel Grades | Special Steel | Z8CDF19-02 | AFNOR | France | Hot-Rolled stainless steel bar and wire rod (NF A 35-574 (1990)) |
| Z20C13 |
|||||
| Z20CN24-13 |
|||||
| Z33C13 |
|||||
| Z44C14 |
|||||
| Z50C15 |
|||||
| Z50CD15 |
|||||
| Z70C15 |
|||||
| Z7CND17-12-02 |
|||||
| Z7CND18-12-03 |
|||||
| Z7CNU16-04 |
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) |
|---|---|---|---|---|---|---|---|
| Max 0.08 | Max 1.00 | Max 2.50 | Max 0.040 | 0.15-0.25 | 17.5-19.5 | Max 0.75 | 1.50-2.50 |
| Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
|---|---|---|---|---|---|---|
| 132 (≥) | 217 (≥) | 14 | 14 | 24 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 344 |
| Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
|---|---|---|---|---|---|---|---|
| 13 | - | - | 0.31 | - | |||
| 199 | 268 | - | 11.3 | 244 | - | ||
| 396 | - | 33 | 41.2 | 424 | 124 |
Heat treated : 1266°C - 1665°C
| Grade | Standard | Country | Application |
|---|---|---|---|
| Z8CDF19-02 | AFNOR | France | Hot-Rolled stainless steel bar and wire rod (NF A 35-574 (1990)) |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com