France AFNOR Z7CND17-12-02 Hot-Rolled stainless steel bar and wire rod (NF A 35-574 (1990)) and Z7CND17-12-02 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Special Steel | Z7CND17-12-02 | AFNOR | France | Hot-Rolled stainless steel bar and wire rod (NF A 35-574 (1990)) | 
| Z13C13 | |||||
| Z15CNS25-20 | |||||
| Z17CNS20-12 | |||||
| Z20C13 | |||||
| Z20CN24-13 | |||||
| Z33C13 | |||||
| Z44C14 | |||||
| Z50C15 | |||||
| Z50CD15 | |||||
| Z70C15 | 
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) | 
|---|---|---|---|---|---|---|---|
| Max 0.07 | Max 0.75 | Max 2.00 | Max 0.040 | 0.015-0.030 | 16.5-18.5 | 10.5-12.5 | 2.00-2.50 | 
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 392 (≥) | 126 (≥) | 42 | 21 | 23 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 424 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 23 | - | - | 0.11 | - | |||
| 345 | 368 | - | 11.3 | 231 | - | ||
| 151 | - | 34 | 21.2 | 124 | 314 | 
Heat treated : 1915°C - 1841°C
| Grade | Standard | Country | Application | 
|---|---|---|---|
| Z7CND17-12-02 | AFNOR | France | Hot-Rolled stainless steel bar and wire rod (NF A 35-574 (1990)) | 