France AFNOR Z6CNDNb18-12 Stainless steel palte & Steel Strip and Z6CNDNb18-12 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Special Steel | Z6CNDNb18-12 | AFNOR | France | Stainless steel palte & Steel Strip | 
| X2CrNiMoN22-5-3 | |||||
| 1.4462(AFNOR) | |||||
| X2CrNiMoCuN25-6-3 | |||||
| 1.4507(AFNOR) | |||||
| 1.4507(AFNOR) | |||||
| X2CrNiMoN25-7-4 | |||||
| 1.4410(AFNOR) | |||||
| X2CrNiMoCuWN25-7-4 | |||||
| 1.4501(AFNOR) | |||||
| Z6CNDNb17-12 | 
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) | Other(%) | 
|---|---|---|---|---|---|---|---|---|
| Max 0.06 | Max 0.75 | Max 2.00 | Max 0.040 | Max 0.015 | 16.5-18.5 | 11.0-13.0 | 2.50-3.00 | Nb+Ta 10xC Max 0.70 | 
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 769 (≥) | 553 (≥) | 32 | 33 | 33 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 442 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 24 | - | - | 0.23 | - | |||
| 814 | 886 | - | 13.3 | 434 | - | ||
| 368 | - | 22 | 42.2 | 222 | 113 | 
Heat treated : 1147°C - 1717°C
| Grade | Standard | Country | Application | 
|---|---|---|---|
| Z6CNDNb18-12 | AFNOR | France | Stainless steel palte & Steel Strip | 