France AFNOR Z15CN16.02CI Cutlery stainless steel and Z15CN16.02CI Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Special Steel | Z15CN16.02CI | AFNOR | France | Cutlery stainless steel | 
| Z4CND17-11-02FF | |||||
| Z4CNU19-09FF | |||||
| Z4CNUD17-11-03FF | |||||
| Z5CN18-11FF | |||||
| Z6CND17-11-02FF | |||||
| Z8C13FF | |||||
| Z8NCTDV25-15BFF | |||||
| Z8C17CI | |||||
| Z11CN18.08CI | |||||
| Z13C13CI | 
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | 
|---|---|---|---|---|---|---|
| 0.15-0.20 | Max 1.00 | Max 1.00 | Max 0.040 | Max 0.015 | 15.5-17.0 | 1.50-2.50 | 
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 924 (≥) | 712 (≥) | 14 | 33 | 24 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 414 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 31 | - | - | 0.44 | - | |||
| 398 | 242 | - | 13.3 | 232 | - | ||
| 121 | - | 13 | 23.2 | 311 | 411 | 
Heat treated : 1721°C - 1551°C
| Grade | Standard | Country | Application | 
|---|---|---|---|
| Z15CN16.02CI | AFNOR | France | Cutlery stainless steel | 
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com