Japan JIS SUS409LTP ferritic stainless steel and SUS409LTP Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Special Steel | SUS409LTP | JIS | Japan | ferritic stainless steel | 
| SUS317LTP | |||||
| SUS3386LTP | |||||
| SUS890LTP | |||||
| SUS321LTP | |||||
| SUS321HTP | |||||
| SUS347TP | |||||
| SUS347HTP | |||||
| SUS329JITP | |||||
| SUS329J4LTP | |||||
| SUS405TP | 
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ti(%) | 
|---|---|---|---|---|---|---|
| Max 0.03 | Max 1.00 | Max 1.00 | Max 0.04 | Max 0.03 | l0.50-17.75 | 6×C%-0.75 | 
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 725 (≥) | 798 (≥) | 31 | 22 | 22 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 221 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 34 | - | - | 0.41 | - | |||
| 793 | 772 | - | 14.3 | 233 | - | ||
| 924 | - | 12 | 41.2 | 332 | 442 | 
Heat treated : 1434°C - 1739°C