Euronorm EN EN X6CrNiMoTiB17-13 Euronorm Stainless Steel and EN X6CrNiMoTiB17-13 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Special Steel | EN X6CrNiMoTiB17-13 | EN | Euronorm | Euronorm Stainless Steel | 
| EN NiCr20TiAl | |||||
| EN NiCr22Fe18Mo | |||||
| EN NiCr23Co12Mo | |||||
| EN NiCr25Co20TiMo | |||||
| EN NiCr25FeAlY | |||||
| EN NiCr26MoW | |||||
| EN NiCr29Fe | |||||
| EN X3CrNiMoBNi7-13-3 | |||||
| EN X5NiCrAlTi31-20 | |||||
| EN X6CrNiMo17-12-2 | 
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) | Ti(%) | 
|---|---|---|---|---|---|---|---|---|
| 0.04-0.08 | 0.75 | 2.00 | 0.035 | 0.015 | 16.0-18.0 | 12.0-.14.0 | 2.00-2.50 | 5XCMax 0.S0 | 
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 266 (≥) | 569 (≥) | 14 | 23 | 22 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 223 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 24 | - | - | 0.23 | - | |||
| 337 | 993 | - | 44.3 | 441 | - | ||
| 853 | - | 23 | 11.2 | 442 | 321 | 
Heat treated : 1698°C - 1663°C
| Grade | Standard | Country | Application | 
|---|---|---|---|
| EN X6CrNiMoTiB17-13 | EN | Euronorm | Euronorm Stainless Steel | 
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...