Germany DIN 1.4935 The high-temperature and high-strength steel and 1.4935 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Special Steel | 1.4935 | DIN | Germany | The high-temperature and high-strength steel | 
| NiFe25Cr20NbTi | |||||
| 2.4955 | |||||
| 65Si7 | |||||
| 1.5028 | |||||
| 1.5028 | |||||
| 37MnSi5 | |||||
| 37MnSi5 | |||||
| X22CrMoV12-1 | |||||
| 1.4923 | |||||
| 1.4934 | 
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) | V(%) | W(%) | 
|---|---|---|---|---|---|---|---|---|---|
| 0.17-0.25 | 0.10-0.50 | 0.30-0.80 | Max 0.045 | Max 0.030 | 11.0-12.5 | 0.30-0.80 | 0.80-1.20 | 0.40-0.60 | 0.40-0.60 | 
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 282 (≥) | 391 (≥) | 32 | 34 | 14 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 433 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 34 | - | - | 0.41 | - | |||
| 524 | 965 | - | 34.3 | 122 | - | ||
| 563 | - | 23 | 11.2 | 211 | 123 | 
Heat treated : 1665°C - 1159°C