France AFNOR 1.4520 Ferritic and 1.4520 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Special Steel | 1.4520 | AFNOR | France | Ferritic | 
| X6CrAl13 | |||||
| 1.4002 | |||||
| X6Cr17 | |||||
| 1.4016 | |||||
| 1.4510 | |||||
| 1.4511 | |||||
| X6CrMo17-1 | |||||
| 1.4113 | |||||
| 1.4521 | |||||
| X2CiTi17 | 
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | N(%) | Ti(%) | 
|---|---|---|---|---|---|---|---|
| Max 0.025 | Max 0.50 | Max 0.50 | Max 0.040 | Max 0.015 | 16.00-18.00 | Max 0.015 | 0.30-0.60 | 
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 925 (≥) | 247 (≥) | 44 | 44 | 11 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 244 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 21 | - | - | 0.44 | - | |||
| 416 | 225 | - | 34.3 | 231 | - | ||
| 695 | - | 14 | 23.2 | 134 | 122 | 
Heat treated : 1612°C - 1821°C
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com