Germany DIN X18CrN28 Stainless steel and X18CrN28 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Special Steel | X18CrN28 | DIN | Germany | Stainless steel | 
| 1.4712 | |||||
| X10CrSi6 | |||||
| X10CrAISi7/X10CrAI7 | |||||
| 1.4713 | |||||
| X7CrTi12 | |||||
| 1.4720 | |||||
| 1.4724 | |||||
| X10CrAISi13/X10CrAI13 | |||||
| 1.4742 | |||||
| X10CrAISi18/X10CrAI18 | 
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | N(%) | 
|---|---|---|---|---|---|---|
| 0.15-0.20 | Max 1.00 | Max 1.00 | Max 0.040 | Max 0.015 | 26.0-29.0 | 0.15-0.25 | 
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 297 (≥) | 787 (≥) | 23 | 31 | 44 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 343 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 23 | - | - | 0.43 | - | |||
| 316 | 153 | - | 31.3 | 322 | - | ||
| 542 | - | 31 | 11.2 | 344 | 122 | 
Heat treated : 1225°C - 1167°C
| Grade | Standard | Country | Application | 
|---|---|---|---|
| X18CrN28 | DIN | Germany | Stainless steel | 
| EN X18CrN28 | EN | Euronorm | Euronorm Stainless Steel | 
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com