China GBT NS313 Nickel-base corrosion-resistant alloy and NS313 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Special Alloy | NS313 | GBT | China | Nickel-base corrosion-resistant alloy | 
| DZ5 | |||||
| NS111 | |||||
| NS112 | |||||
| NS113 | |||||
| NS131 | |||||
| NS141 | |||||
| NS142 | |||||
| NS143 | |||||
| NS311 | |||||
| NS312 | 
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Cu(%) | Al(%) | Fe(%) | 
|---|---|---|---|---|---|---|---|---|---|
| Max 0.10 | Max 0.05 | Max 1.00 | Max 0.030 | Max 0.015 | 21.0-25.0 | Balance | Max 1.00 | 1.00-1.70 | 10.0-15.0 | 
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 737 (≥) | 473 (≥) | 31 | 33 | 41 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 431 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 11 | - | - | 0.34 | - | |||
| 389 | 832 | - | 33.3 | 131 | - | ||
| 124 | - | 42 | 43.2 | 242 | 414 | 
Heat treated : 1565°C - 1593°C