SCMnCr4 Mould Steel and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Mould Steel | SCMnCr4 | |||
| SCW63 | |||||
| SCC3 | |||||
| SCC5 | |||||
| SCMn1 | |||||
| SCMn2 | |||||
| SCMn3 | |||||
| SCMn5 | |||||
| SCSiMn2 | |||||
| SCMnCr2 | |||||
| SCMnCr3 | 
| C ≤ | Si ≤ | Mn ≤ | P ≤ | S ≤ | Cr | Ni | 
|---|---|---|---|---|---|---|
| 0.35-0.45 | 0.3-0.6 | 1.2-1.6 | 0.04 | 0.04 | 0.4-0.8 | |
| Mo | Al | Cu | Nb | Ti | V | Ce | 
| N | Co | Pb | B | Other | ||
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 974 (≥) | 744 (≥) | 32 | 44 | 21 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 222 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 23 | - | - | 0.33 | - | |||
| 131 | 289 | - | 24.3 | 243 | - | ||
| 473 | - | 42 | 11.2 | 114 | 443 | 
Heat treated : 1287°C - 1814°C