GS-40CrNiMo6-5-6 Mould Steel and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Mould Steel | GS-40CrNiMo6-5-6 | |||
| G34CrNiMo6 | |||||
| 1.6582 | |||||
| GS-34CrNiMo6 | |||||
| 1.6582 | |||||
| G33CrNiMo7-4-4 | |||||
| 1.6740 | |||||
| GS-33CrNiMo7-4-4 | |||||
| 1.6740 | |||||
| GS-38CrNiMo8-4-4 | |||||
| 1.6741 | 
| C ≤ | Si ≤ | Mn ≤ | P ≤ | S ≤ | Cr | Ni | 
|---|---|---|---|---|---|---|
| 0.37-0.44 | 0.30-0.60 | 0.60-1.00 | 0.025 | 0.025 | 1.10-1.50 | 1.30-1.70 | 
| Mo | Al | Cu | Nb | Ti | V | Ce | 
| 0.50-0.70 | ||||||
| N | Co | Pb | B | Other | ||
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 734 (≥) | 753 (≥) | 42 | 31 | 44 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 424 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 22 | - | - | 0.21 | - | |||
| 661 | 967 | - | 24.3 | 431 | - | ||
| 633 | - | 23 | 33.2 | 223 | 323 | 
Heat treated : 1775°C - 1992°C
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...