GGG-Ni22 Mould Steel and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Mould Steel | GGG-Ni22 | |||
| GGG-NiMn13-7 | 
                                |||||
| 0.7652 | 
                                |||||
| GGG-NiCrNb20-2 | 
                                |||||
| 0.7659 | 
                                |||||
| GGG-NiCr20-2 | 
                                |||||
| 0.7660 | 
                                |||||
| GGG-NiCr20-3 | 
                                |||||
| 0.7661 | 
                                |||||
| GGG-NiSiCr20-5-2 | 
                                |||||
| 0.7665 | 
                                
| 
				C ≤  | 
			
				Si ≤  | 
			
				Mn ≤  | 
			
				P ≤  | 
			
				S ≤  | 
			Cr | Ni | 
|---|---|---|---|---|---|---|
| 3.0 | 1.0-3.0 | 1.5-2.5 | 21.0-24.0 | |||
| Mo | Al | Cu | Nb | Ti | V | Ce | 
| N | Co | Pb | B | Other | ||
| Yield Rp0.2 (MPa)  | 
                                            Tensile Rm (MPa)  | 
                                            Impact KV/Ku (J)  | 
                                            Elongation A (%)  | 
                                            Reduction in cross section on fracture Z (%)  | 
                                            As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 635 (≥) | 219 (≥) | 32 | 34 | 22 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 314 | 
| Temperature (°C)  | 
                                        Modulus of elasticity (GPa)  | 
                                        Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C)  | 
                                        Specific thermal capacity (J/kg·°C)  | 
                                        Specific electrical resistivity (Ω mm²/m)  | 
                                        Density (kg/dm³)  | 
                                        Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 11 | - | - | 0.12 | - | |||
| 314 | 916 | - | 14.3 | 134 | - | ||
| 435 | - | 44 | 42.2 | 113 | 234 | 
Heat treated : 1935°C - 1197°C