1.4469 Mould Steel and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Mould Steel | 1.4469 | |||
| 1.4446 | |||||
| GX6CrNiMo17-13 | |||||
| 1.4448 | |||||
| GX6CrNiMo24-8-2 | |||||
| 1.4463 | |||||
| GX40CrNiMo27-5 | |||||
| 1.4464 | |||||
| GX2CrNiMoN25-6-3 | |||||
| 1.4468 | |||||
| GX2CrNiMoN26-7-4 | 
| C ≤ | Si ≤ | Mn ≤ | P ≤ | S ≤ | Cr | Ni | 
|---|---|---|---|---|---|---|
| 0.03 | 1.00 | 1.00 | 0.035 | 0.025 | 25.0-27.0 | 6.00-8.00 | 
| Mo | Al | Cu | Nb | Ti | V | Ce | 
| 3.00-5.00 | ≤1.30 | |||||
| N | Co | Pb | B | Other | ||
| 0.12-0.25 | ||||||
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 665 (≥) | 142 (≥) | 34 | 42 | 12 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 322 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 12 | - | - | 0.14 | - | |||
| 317 | 672 | - | 13.3 | 213 | - | ||
| 583 | - | 32 | 44.2 | 144 | 312 | 
Heat treated : 1435°C - 1162°C
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com