| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | High Alloy | X6CrNi18-11 | |||
| X19CrMo 12-1 | |||||
| X20CrMoV 12-1 | |||||
| X20CrMoV 11-1 | |||||
| X22CrMoV 12-1 | |||||
| X20CrMoWV 12-1 | |||||
| X12CrNiMoV 12-3 | |||||
| X11CrNiMoN 12 | |||||
| X6CrNiTiB 18-10 | |||||
| X8CrNiTi 18-10 | |||||
| X6CrNiWNb16-16 | 
| C | Si ≤ | Mn ≤ | P ≤ | S ≤ | Cr | Ni | Mo | Other | 
|---|---|---|---|---|---|---|---|---|
| 0.04-0.08 | 0.75 | 2.00 | 0.035 | 0.015 | 17.0-19.0 | 10.0-12.0 | ----------- | N ≤0.11 | 
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 715 (≥) | 836 (≥) | 44 | 32 | 32 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 434 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 12 | - | - | 0.44 | - | |||
| 357 | 325 | - | 21.3 | 114 | - | ||
| 169 | - | 43 | 24.2 | 222 | 312 | 
Heat treated : 1766°C - 1295°C