HNV7 (71360) High Alloy and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | High Alloy | HNV7 (71360) | |||
| S64005 | |||||
| HNV2 | |||||
| S64006 | |||||
| HNV3 | |||||
| S65007 | |||||
| HNV4 | |||||
| HNV5 | |||||
| S63005 | |||||
| HNV6 | |||||
| S65006 | 
| C ≤ | Si ≤ | Mn ≤ | P ≤ | S ≤ | Cr | Ni | 
|---|---|---|---|---|---|---|
| 0.55 | 0.20 | 00.20 | 3.50 | |||
| Mo | Al | Cu | Nb | Ti | V | Ce | 
| N | Co | Pb | B | Other | ||
| W 14.0 | ||||||
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 425 (≥) | 759 (≥) | 32 | 22 | 24 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 423 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 34 | - | - | 0.32 | - | |||
| 462 | 977 | - | 43.3 | 221 | - | ||
| 373 | - | 43 | 12.2 | 214 | 434 | 
Heat treated : 1666°C - 1463°C
| Grade | Standard | Country | Application | 
|---|---|---|---|
| SAE HNV7(71360) | SAE | USA | precipitation hardening | 
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com