24CrMoV5-5 High Alloy and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | High Alloy | 24CrMoV5-5 | |||
| 11CrMo9-10 | |||||
| 1.7383 | |||||
| 14MoV6-3 | |||||
| 1.7715 | |||||
| 21MoV5-3 | |||||
| 1.5404 | |||||
| 17MoV8-4 | |||||
| 1.5406 | |||||
| 40CrMoV4-6 | |||||
| 1.7711 | 
| C ≤ | Si ≤ | Mn ≤ | P ≤ | S ≤ | Cr | Ni | 
|---|---|---|---|---|---|---|
| 0.20-0.28 | 0.15-0.35 | 0.30-0.60 | 0.035 | 0.035 | 1.20-1.50 | ≤0.60 | 
| Mo | Al | Cu | Nb | Ti | V | Ce | 
| 0.50-0.60 | 0.15-0.25 | |||||
| N | Co | Pb | B | Other | ||
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 988 (≥) | 756 (≥) | 23 | 32 | 11 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 333 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 11 | - | - | 0.23 | - | |||
| 285 | 116 | - | 41.3 | 433 | - | ||
| 799 | - | 24 | 44.2 | 313 | 411 | 
Heat treated : 1166°C - 1536°C
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...