2304 High Alloy and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | High Alloy | 2304 | |||
| S38815 | |||||
| S31200 | |||||
| S31260 | |||||
| S31803 | |||||
| S32001 | |||||
| S32003 | |||||
| S32101 | |||||
| S32205 | |||||
| 2205 | |||||
| S32304 | 
| C ≤ | Si ≤ | Mn ≤ | P ≤ | S ≤ | Cr | Ni | 
|---|---|---|---|---|---|---|
| 0.03 | 1 | 2.5 | 0.04 | 0.03 | 21.5-24.5 | 3-5.5 | 
| Mo | Al | Cu | Nb | Ti | V | Ce | 
| 0.05-0.6 | 0.05-0.6 | |||||
| N | Co | Pb | B | Other | ||
| 0.05-0.2 | ||||||
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 973 (≥) | 293 (≥) | 42 | 44 | 23 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 234 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 24 | - | - | 0.14 | - | |||
| 781 | 527 | - | 21.3 | 222 | - | ||
| 586 | - | 33 | 12.2 | 244 | 432 | 
Heat treated : 1258°C - 1892°C
| Grade | Standard | Country | Application | 
|---|---|---|---|
| S32304 | UNS | USA | Dual-phase steel | 
| S32304 | UNS | USA | Dual-phase steel | 
| 2304 | UNS | USA | Dual-phase steel | 
| 2304 | UNS | USA | Dual-phase steel | 
| SS 2304 | SS | Sweden | Swedish SS standard stainless steel and heat resistant steel | 
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...