1.4934 High Alloy and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | High Alloy | 1.4934 | |||
| 2.4816 | |||||
| 1.4910 | |||||
| 1.4911 | |||||
| 1.4913 | |||||
| 1.4914 | |||||
| 1.4919 | |||||
| 1.4920 | |||||
| 1.4921 | |||||
| 1.4922 | |||||
| 1.4923 | 
| C | Si ≤ | Mn ≤ | P ≤ | S ≤ | Cr | Ni | Mo | Other | 
|---|---|---|---|---|---|---|---|---|
| 0.18-0.24 | 0.18-0.24 | 0.40-0.90 | 0.025 | 0.015 | 11.0-12.5 | 0.30-0.80 | 0.80-1.20 | V 0.25-0.35 | 
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 763 (≥) | 998 (≥) | 11 | 14 | 44 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 234 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 31 | - | - | 0.32 | - | |||
| 559 | 965 | - | 31.3 | 144 | - | ||
| 594 | - | 44 | 11.2 | 413 | 424 | 
Heat treated : 1169°C - 1478°C