SN490B Carbon Steel and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Carbon Steel | SN490B | |||
| SNB5 | 
                                |||||
| SNB7 | 
                                |||||
| SNB16 | 
                                |||||
| SNB21-1~5 | 
                                |||||
| SNB22-1~5 | 
                                |||||
| SNB23-1~5 | 
                                |||||
| SNB24-1~5 | 
                                |||||
| SN400A | 
                                |||||
| SN400B | 
                                |||||
| SN400C | 
                                
| 
				C ≤  | 
			
				Si ≤  | 
			
				Mn ≤  | 
			
				P ≤  | 
			
				S ≤  | 
			Cr | Ni | 
|---|---|---|---|---|---|---|
| 0.18-0.22 | 0.55 | 1.6 | 0.03 | 0.015 | ||
| Mo | Al | Cu | Nb | Ti | V | Ce | 
| 0.44-0.46 | ||||||
| N | Co | Pb | B | Other | ||
| Thickness 6~100/mm | ||||||
| Yield Rp0.2 (MPa)  | 
                                            Tensile Rm (MPa)  | 
                                            Impact KV/Ku (J)  | 
                                            Elongation A (%)  | 
                                            Reduction in cross section on fracture Z (%)  | 
                                            As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 762 (≥) | 658 (≥) | 31 | 11 | 13 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 222 | 
| Temperature (°C)  | 
                                        Modulus of elasticity (GPa)  | 
                                        Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C)  | 
                                        Specific thermal capacity (J/kg·°C)  | 
                                        Specific electrical resistivity (Ω mm²/m)  | 
                                        Density (kg/dm³)  | 
                                        Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 34 | - | - | 0.14 | - | |||
| 752 | 727 | - | 12.3 | 231 | - | ||
| 722 | - | 21 | 43.2 | 243 | 221 | 
Heat treated : 1616°C - 1868°C