29Cr-9Ni+ Carbon Steel and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Carbon Steel | 29Cr-9Ni+ | |||
| ASTM   HH | |||||
| UNS   J93503 | |||||
| ASTM   HI | |||||
| UNS   J94003 | |||||
| 28Cr-15Ni | |||||
| ASTM   HK | |||||
| UNS   J94224 | |||||
| 25Cr-20Ni+ | |||||
| ASTM   HE | |||||
| UNS   J93403 | 
| C ≤ | Si ≤ | Mn ≤ | P ≤ | S ≤ | Cr | Ni | 
|---|---|---|---|---|---|---|
| 0.2-0.5 | 2.0 | 2.0 | 0.04 | 0.04 | 26.0-30.0 | 8.0-11.0 | 
| Mo | Al | Cu | Nb | Ti | V | Ce | 
| ≤0.5 | ||||||
| N | Co | Pb | B | Other | ||
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 663 (≥) | 127 (≥) | 34 | 42 | 32 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 241 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 13 | - | - | 0.33 | - | |||
| 469 | 774 | - | 31.3 | 123 | - | ||
| 561 | - | 31 | 14.2 | 343 | 311 | 
Heat treated : 1295°C - 1875°C
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com