Chemical composition(mass fraction)(wt.%) of the C96200

Element Min Max Similar

Mechanical Properties of steel grade C96200

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV/Ku (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
365 (≥) 458 (≥) 21 14 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 412

Physical Properties of steel grade C96200

Temperature
(°C)
Modulus of elasticity
(GPa)
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and Thermal conductivity
(W/m·°C)
Specific thermal capacity
(J/kg·°C)
Specific electrical resistivity
(Ω mm²/m)
Density
(kg/dm³)
Poisson’s coefficient, ν
31 - -     0.11 -  
829 848 - 43.3 341   -  
288 - 23 21.2   141 333

Heat Treatment of steel grade C96200

Heat treated : 1116°C - 1797°C

Technological Curves of steel grade C96200

Cross Reference Table (Equivalent Grade) of C96200

Available Suppliers

Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...

Rfq.: sales@longhaisteel.com
  • Do you supply this C96200?
  • List your company on S&G now? Join
  • Non-paying users only
Sidebar RFQs Menu My Account
Top