Available 24/7 at contact@steel-grades.com

NBR 7837 Class Ⅱ C

Brazil NBR NBR7837ClassⅡC Cast iron parts for use in temperatures above 760℃ and Mechanical Properties, Chemical Element, Cross Reference.

Category Grade Standard Region/Area Standard Content
Metals NBR 7837 Class Ⅱ C ABNT NBR 7837 Brazil Cast iron parts for use in temperatures above 760℃

Chemical composition(mass fraction)(wt.%) of the NBR 7837 Class Ⅱ C

Element Min Max Similar
C 1.8000 2.6000 -
Mn 0.4000 1.0000 -
P - - 0.2000
S - - 0.1500
Si 5.0000 6.0000 -
Ni 13.0000 32.0000 -
Cr 1.8000 5.5000 -
Mo - 1.0000 -
Cu - 10.0000 -

Mechanical Properties of steel grade NBR 7837 Class Ⅱ C

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV/Ku (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
858 (≥) 131 (≥) 31 44 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 134

Physical Properties of steel grade NBR 7837 Class Ⅱ C

Temperature
(°C)
Modulus of elasticity
(GPa)
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and Thermal conductivity
(W/m·°C)
Specific thermal capacity
(J/kg·°C)
Specific electrical resistivity
(Ω mm²/m)
Density
(kg/dm³)
Poisson’s coefficient, ν
32 - -     0.33 -  
227 112 - 41.3 114   -  
191 - 14 23.2   331 134

Heat Treatment of steel grade NBR 7837 Class Ⅱ C

Heat treated : 1973°C - 1983°C

Technological Curves of steel grade NBR 7837 Class Ⅱ C

Cross Reference Table (Equivalent Grade) of NBR 7837 Class Ⅱ C

Available Suppliers

Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...

Rfq.: sales@longhaisteel.com
  • Do you supply this NBR 7837 Class Ⅱ C?
  • List your company on S&G now? Join
  • Non-paying users only
Sidebar RFQs Menu My Account
Top