Outokumpu 347

Global 企业标准 Outokumpu347 and Mechanical Properties, Chemical Element, Cross Reference.

Datasheet for: Metals: Outokumpu347 / Outokumpu 347
Category Grade Standard Region/Area Standard Content
Metals Outokumpu 347 -- Global

Chemical composition(mass fraction)(wt.%) of the Outokumpu 347

Element Min Max Similar
Other - - -
Ni - 9.1000 -
N - 0.0400 -
Cr - 17.3000 -
C - 0.0400 -

Mechanical Properties of steel grade Outokumpu 347

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV/Ku (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
563 (≥) 137 (≥) 11 11 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 144

Physical Properties of steel grade Outokumpu 347

Temperature
(°C)
Modulus of elasticity
(GPa)
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and Thermal conductivity
(W/m·°C)
Specific thermal capacity
(J/kg·°C)
Specific electrical resistivity
(Ω mm²/m)
Density
(kg/dm³)
Poisson’s coefficient, ν
33 - -     0.31 -  
819 526 - 32.3 423   -  
637 - 33 32.2   331 342

Heat Treatment of steel grade Outokumpu 347

Heat treated : 1399°C - 1216°C

Technological Curves of steel grade Outokumpu 347

Cross Reference Table (Equivalent Grade) of Outokumpu 347

Available Suppliers

Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...

Rfq.: sales@longhaisteel.com
  • Do you supply this Outokumpu 347?
  • List your company on S&G now? Join
  • Non-paying users only
Sidebar RFQs Menu My Account
Top