Soldur 260

Global 企业标准 Soldur260 and Mechanical Properties, Chemical Element, Cross Reference.

Datasheet for: Metals: Soldur260 / Soldur 260
Category Grade Standard Region/Area Standard Content
Metals Soldur 260 -- Global

Chemical composition(mass fraction)(wt.%) of the Soldur 260

Element Min Max Similar
Ti - 0.1500 -
Si - 0.0500 -
S - 0.0250 -
P - 0.0250 -
Nb - 0.0900 -
Mn - 0.6000 -
C - 0.1000 -
Al 0.0150 - -

Mechanical Properties of steel grade Soldur 260

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV/Ku (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
582 (≥) 325 (≥) 44 13 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 223

Physical Properties of steel grade Soldur 260

Temperature
(°C)
Modulus of elasticity
(GPa)
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and Thermal conductivity
(W/m·°C)
Specific thermal capacity
(J/kg·°C)
Specific electrical resistivity
(Ω mm²/m)
Density
(kg/dm³)
Poisson’s coefficient, ν
22 - -     0.34 -  
497 667 - 11.3 213   -  
183 - 14 33.2   144 141

Heat Treatment of steel grade Soldur 260

Heat treated : 1234°C - 1519°C

Technological Curves of steel grade Soldur 260

Cross Reference Table (Equivalent Grade) of Soldur 260

Available Suppliers

Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...

Rfq.: sales@longhaisteel.com
  • Do you supply this Soldur 260?
  • List your company on S&G now? Join
  • Non-paying users only
Sidebar RFQs Menu My Account
Top