England B.S. TA6 Specification for sheet and strip of commercially pure titanium (tensile strength 570-730 N/mm2) and Mechanical Properties, Chemical Element, Cross Reference.

Datasheet for: Metals: TA6 / TA 6
Category Grade Standard Region/Area Standard Content
Metals TA 6 BS 2TA 6 England Specification for sheet and strip of commercially pure titanium (tensile strength 570-730 N/mm2)

Chemical composition(mass fraction)(wt.%) of the TA 6

Element Min Max Similar
Ti - - -
H - 0.1250 -
Fe - 0.2000 -

Mechanical Properties of steel grade TA 6

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV/Ku (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
284 (≥) 529 (≥) 43 33 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 432

Physical Properties of steel grade TA 6

Temperature
(°C)
Modulus of elasticity
(GPa)
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and Thermal conductivity
(W/m·°C)
Specific thermal capacity
(J/kg·°C)
Specific electrical resistivity
(Ω mm²/m)
Density
(kg/dm³)
Poisson’s coefficient, ν
32 - -     0.11 -  
888 711 - 22.3 411   -  
447 - 22 31.2   123 224

Heat Treatment of steel grade TA 6

Heat treated : 1791°C - 1466°C

Technological Curves of steel grade TA 6

Cross Reference Table (Equivalent Grade) of TA 6

Available Suppliers

Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...

Rfq.: sales@longhaisteel.com
  • Do you supply this TA 6?
  • List your company on S&G now? Join
  • Non-paying users only
Sidebar RFQs Menu My Account
Top