USA ASTM CW-12MW Castings, Nickel and Nickel Alloy and CW-12MW Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application |
|---|---|---|---|---|---|
| Steel Grades | Special Alloy | CW-12MW | ASTM | USA | Castings, Nickel and Nickel Alloy |
| J93254 |
|||||
| CZ-100 |
|||||
| M-35-1 |
|||||
| M-35-2 |
|||||
| M-30H |
|||||
| M-25S |
|||||
| M-30C |
|||||
| N-12MV |
|||||
| N-7M |
|||||
| CY-40 |
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) | V(%) | W(%) | Fe(%) |
|---|---|---|---|---|---|---|---|---|---|---|
| 0.12 | 1 | 1 | 0.04 | 0.03 | 15.5-17.5 | Bal | 16.0-18.0 | 0.20-0.40 | 3.75-5.25 | 4.5-7.5 |
| Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
|---|---|---|---|---|---|---|
| 227 (≥) | 447 (≥) | 41 | 21 | 13 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 234 |
| Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
|---|---|---|---|---|---|---|---|
| 21 | - | - | 0.34 | - | |||
| 119 | 715 | - | 33.3 | 241 | - | ||
| 813 | - | 33 | 22.2 | 243 | 332 |
Heat treated : 1845°C - 1818°C
| Grade | Standard | Country | Application |
|---|---|---|---|
| CW-12MW | AISI | USA | |
| CW-12MW | ASTM | USA | Castings, Nickel and Nickel Alloy |
| CW-12MW | ASTM | USA | Castings, Nickel and Nickel Alloy |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com