USA AISI 19Cr-11Ni+Mo and 19Cr-11Ni+Mo Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application |
|---|---|---|---|---|---|
| Steel Grades | Special Alloy | 19Cr-11Ni+Mo | AISI | USA | |
| UNS J92900 |
|||||
| 19Cr-10Ni+Mo |
|||||
| 19Cr-10Ni+Nb |
|||||
| UNS J92710 |
|||||
| ASTM CF-8C |
|||||
| 19Cr-11Ni+Mo |
|||||
| UNS J92999 |
|||||
| ASTM CG-3M |
|||||
| ASTM CG-8M |
|||||
| UNS J93000 |
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) |
|---|---|---|---|---|---|---|---|
| Max 0.08 | Max 0.50 | Max 1.50 | Max 0.04 | Max 0.040 | 18.0-21.0 | 9.0-13.0 | 3.0-4.0 |
| Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
|---|---|---|---|---|---|---|
| 688 (≥) | 312 (≥) | 34 | 22 | 23 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 324 |
| Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
|---|---|---|---|---|---|---|---|
| 32 | - | - | 0.24 | - | |||
| 438 | 763 | - | 22.3 | 424 | - | ||
| 482 | - | 12 | 31.2 | 423 | 222 |
Heat treated : 1342°C - 1915°C
| Grade | Standard | Country | Application |
|---|---|---|---|
| 19Cr-11Ni+Mo | AISI | USA | |
| 19Cr-11Ni+Mo | AISI | USA | |
| 19Cr-11Ni+Mo | AISI | USA | |
| 19Cr-11Ni+Mo | AISI | USA | |
| 19Cr-11Ni+Mo | AISI | USA |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com