07X16H6 Austenitic - Martensitic steel and 07X16H6 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Heat-Resistant Steel | 07X16H6 | Austenitic - Martensitic steel | ||
| 14X17H2 | |||||
| 10X13Ю | |||||
| 08X13 | |||||
| 12X17 | |||||
| 08X17T | |||||
| 15X18Ю | |||||
| 15X25T | |||||
| 15X28 | |||||
| 20X13H4Γ9 | |||||
| 09X15H8Ю | 
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) | W(%) | Ti(%) | 
|---|---|---|---|---|---|---|---|---|---|
| 0.05-0.09 | Max 0.80 | Max 0.80 | Max 0.035 | Max 0.025 | 15.5-17.5 | 5.00-8.00 | Max 0.30 | Max 0.20 | Max 0.2 | 
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 667 (≥) | 235 (≥) | 12 | 23 | 21 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 422 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 34 | - | - | 0.44 | - | |||
| 572 | 873 | - | 24.3 | 341 | - | ||
| 495 | - | 14 | 43.2 | 211 | 211 | 
Heat treated : 1882°C - 1869°C
| Grade | Standard | Country | Application | 
|---|---|---|---|
| 07X16H6 | Austenitic - Martensitic steel | 
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com