USA AMS AMS 5411, Inconel 722 Superalloys Used for gas turbine structural components, such as turbine section frames. The alloy is useful where oxidation resistance and high temperature strength are of major importance. and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Class | Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Superalloys | Inconel 722 | AMS | USA | Used for gas turbine structural components, such as turbine section frames. The alloy is useful where oxidation resistance and high temperature strength are of major importance. |
C | Si | Mn | Cr | Ni | Cu | Fe | P | S | Ti | Al |
---|---|---|---|---|---|---|---|---|---|---|
≤0.08 | ≤0.07 | ≤1.00 | 14.00 -17.00 | ≤Balance | ≤0.5 | 5.00 -9.00 | ≤ ≥ | ≤0.01 | 2 -2.75 | 0.40 -1.00 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
923 (≥) | 188 (≥) | 31 | 32 | 13 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 224 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
14 | - | - | 0.13 | - | |||
387 | 446 | - | 34.3 | 414 | - | ||
559 | - | 31 | 32.2 | 344 | 413 |
Heat treated : 1325°C - 1629°C
Grade | Standard | Country | Application |
---|---|---|---|
1.7220 | |||
1.7223 | |||
1.7225 | |||
1.7227 | |||
1.7228 | |||
1.0722 | |||
1.7227 | |||
1.7221 | |||
1.7220 | |||
1.7221 | |||
1.7221 | |||
1.7225 | |||
INCONEL alloy 722 | |||
3.7225 Ti Alloy | |||
SS 2722 | |||
DIN 1.7220 | |||
DIN 1.7223 | |||
DIN 1.7225 | |||
DIN 1.7228 | |||
SS14:2722 |
AMS 5411 | Nickel Inconel 722 AMS 5541 Strip | AMS-5411.pdf |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com