NIMONIC® alloy 105

USA SMC SMC-081 NIMONIC® alloy 105 NIMONIC® alloy 105 and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.

SMC NIMONIC® alloy 105 SMC NIMONIC® alloy 105 Datasheet
Category Class Grade Standard Country Application
Steel GradesSuperalloys NIMONIC® alloy 105 SMC USA NIMONIC® alloy 105
Datasheet for:Steel Grades:Superalloys:NIMONIC® alloy 105

Chemical composition(mass fraction)(wt.%) of the NIMONIC® alloy 105

Elements Min.(≥) Max.(≤)
C - 0.17
Si - 1.00
Cu - 0.20
Fe - 1.00
Mn - 1.00
Cr 14.00 15.70
Ti 0.90 1.50
Al 4.50 4.90
Co 18.00 22.00
Mo 4.50 5.50
Pb - 0.0015
S - 0.0100
B 0.0030 0.0100
Zr - 0.1500
Ni - Balance

Mechanical properties / Mechanische Eigenschaften / Caracteristiques mecaniques of grade NIMONIC® alloy 105

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV/Ku (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
155 (≥) 193 (≥) 24 23 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 133
Temperature
(°C)
Modulus of elasticity
(GPa)
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and Thermal conductivity
(W/m·°C)
Specific thermal capacity
(J/kg·°C)
Specific electrical resistivity
(Ω mm²/m)
Density
(kg/dm³)
Poisson’s coefficient, ν
11 - -     0.34 -  
378 443 - 44.3 442   -  
576 - 41 23.2   232 422
Heat treated : 1967°C - 1341°C
The material does not have direct Metallography properties.
Directory is being updated.
The material does not have direct Metallography properties.
Directory is being updated.
Cross Reference Table(Equivalent Grade)
Grade Standard Country Application
HEV5 UNS USA
Steel for exhaust valves
N07080 AISI USA
Steel for exhaust valves
HEV6 UNS USA
Steel for exhaust valves
N07090 AISI USA
Steel for exhaust valves
NIMONIC® alloy 105 SMC USA
NIMONIC® alloy 105
NIMONIC® alloy 90 SMC USA
NIMONIC® alloy 90 (UNS N07090/W. Nr. 2.4632)
Relevant standard
Standard No. Description Download
SMC-081 NIMONIC® alloy 105 (W. Nr. 2.4634)
Contact Suppliers with your enquiries for NIMONIC® alloy 105 any of the shape and size.

Haihong International Trade (HK) CO., Limited

Stainless Steel, Special Steel, Compressor Blading, Turbine Blading, Superalloy Supplier.
SMC-081, NIMONIC® alloy 105 can be supplied as steel plate/ sheet, round steel bar, steel tube/pipe, steel stripe, steel billet, steel ingot, steel wire rods. electroslag, forged ring/ block,etc.
TEL:+86-816-3646575 FAX: +86-816-3639422
M/B:+86-15386639257
E-mail: [email protected]
Website: https://www.tool-die-steels.com/

Round, Square, Hex, Flat, Hollow

NIMONIC® alloy 105 Bar

Enquiry

Shaft, Ring, Disks, Cylinder

NIMONIC® alloy 105 Forged

Enquiry

Special shaped profile steel

NIMONIC® alloy 105 Steel

Enquiry

High precision machine Forging parts

NIMONIC® alloy 105 Parts

Enquiry
Join Supplier: sal[email protected]