USA ASTM F 688 (2014), F688 R30035 Superalloys Standard Specification for Wrought Cobalt-35Nickel-20Chromium-10Molybdenum Alloy Plate, Sheet, and Foil for Surgical Implants (UNS R30035) and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Class | Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Superalloys | F688 R30035 | ASTM | USA | Standard Specification for Wrought Cobalt-35Nickel-20Chromium-10Molybdenum Alloy Plate, Sheet, and Foil for Surgical Implants (UNS R30035) |
C | P | Si | Ni | Co | Mn | S | Cr | Mo | Ti | Fe |
---|---|---|---|---|---|---|---|---|---|---|
≤0.025 | ≤0.015 | ≤0.15 | 33.00 -37.00 | ≤Bal | ≤0.15 | ≤0.01 | 19.00 -21.00 | 9.00 -10.50 | ≤1.00 | ≤1.00 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
337 (≥) | 811 (≥) | 32 | 24 | 31 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 331 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
13 | - | - | 0.31 | - | |||
354 | 141 | - | 14.3 | 432 | - | ||
292 | - | 13 | 44.2 | 221 | 222 |
Heat treated : 1733°C - 1333°C
F 688 (2014) | Standard Specification for Wrought Cobalt-35Nickel-20Chromium-10Molybdenum Alloy Plate, Sheet, and Foil for Surgical Implants (UNS R30035) | F-688-(2014).pdf |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com