USA SAE SAE AMS 5542N (2007), SAE AMS 5582F (2012), SAE AMS 5598E (2007), SAE AMS 5667N (2015), SAE AMS 5668J (2007), SAE AMS 5669B (1965), SAE AMS 5670F (2005), SAE AMS 5671G (2007), SAE AMS 5698G (2007), SAE AMS 5699G (2007), SAE AMS 5747D (2006), SAE AMS 5779E (2003), SAE AMS 5583E (2013), SAE J 467b (1968), SAE J 470 (1976), Inconel X750 Superalloys Nickel Alloy, Corrosion and Heat-Resistant, Sheet, Strip, and Plate 72Ni - 15.5Cr - 0.95Cb(Nb) - 2.5Ti - 0.70Al - 7.0Fe Annealed and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Class | Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Superalloys | Inconel X750 | SAE | USA | Nickel Alloy, Corrosion and Heat-Resistant, Sheet, Strip, and Plate 72Ni - 15.5Cr - 0.95Cb(Nb) - 2.5Ti - 0.70Al - 7.0Fe Annealed |
C | Mn | Si | S | P | Cu | Fe | Co | Nb | Cr | Ni | Al | Ti |
---|---|---|---|---|---|---|---|---|---|---|---|---|
≤0.08 | ≤1.0 | ≤0.5 | ≤0.01 | ≤0.015 | ≤0.5 | 5.0 -9.0 | ≤1.0 | 0.70 -1.20 | 14.0 -17.0 | 70 - ≥ | 0.40 -1.00 | 2.25 -2.75 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
585 (≥) | 351 (≥) | 11 | 24 | 32 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 241 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
31 | - | - | 0.11 | - | |||
311 | 526 | - | 22.3 | 331 | - | ||
975 | - | 21 | 24.2 | 313 | 123 |
Heat treated : 1673°C - 1355°C
Grade | Standard | Country | Application |
---|---|---|---|
N07750 | |||
N07750 | |||
UNS N07750 | |||
UNS N07750 | |||
INCONEL alloy X-750 | |||
Inconel X-750 | |||
Inconel X-750 |
SAE AMS 5542N (2007) | Nickel Alloy, Corrosion and Heat-Resistant, Sheet, Strip, and Plate 72Ni - 15.5Cr - 0.95Cb(Nb) - 2.5Ti - 0.70Al - 7.0Fe Annealed | SAE-AMS-5542N-(2007).pdf |
SAE AMS 5582F (2012) | Nickel Alloy, Corrosion and Heat-Resistant, Seamless Tubing 72Ni - 15.5Cr - 0.95Cb - 2.5Ti - 0.70Al - 7.0Fe Solution Heat Treated, Precipitation Hardenable to 155 ksi (1069 MPa) Tensile Strength | SAE-AMS-5582F-(2012).pdf |
SAE AMS 5598E (2007) | Nickel Alloy, Corrosion and Heat-Resistant, Sheet, Strip, and Plate 72Ni - 15.5Cr - 0.95 (Cb (Nb) + Ta) - 2.5Ti - 0.70Al - 7.0Fe Consumable Electrode, Remelted or Vacuum Induction Melted, Solution Heat Treated, Precipitation-Hardenable | SAE-AMS-5598E-(2007).pdf |
SAE AMS 5667N (2015) | Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 72Ni - 15.5Cr - 0.95Cb - 2.5Ti - 0.70Al - 7.0Fe Equalized, Precipitation Hardenable | SAE-AMS-5667N-(2015).pdf |
SAE AMS 5668J (2007) | Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 72Ni - 15.5Cr - 7.0Fe - 2.5Ti - 1.0Cb (Nb) - 0.70Al 2100°F (1149°C) Solution and Precipitation Heat Treated | SAE-AMS-5668J-(2007).pdf |
SAE AMS 5669B (1965) | Alloy Bars, Corrosion and Heat Resistant Nickel Base - 15.5Cr - 0.95 (Cb + Ta) - 2.5Ti - 0.70Al - 7.0Fe Consumable Electrode or Vacuum Induction Melted | SAE-AMS-5669B-(1965).pdf |
SAE AMS 5670F (2005) | Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 72Ni - 15.5Cr - 0.95Cb(Nb) - 2.5Ti - 0.70Al - 7.0Fe 1800°F (982°C) Solution Heat Treated, Precipitation-Hardenable | SAE-AMS-5670F-(2005).pdf |
SAE AMS 5671G (2007) | Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 72Ni - 15.5Cr - 0.95Cb - 2.5Ti - 0.70Al - 7.0Fe Consumable Electrode or Vacuum Induction Melted 1800°F (982°C) Solution Heat Treated, Precipitation Hardenable | SAE-AMS-5671G-(2007).pdf |
SAE AMS 5698G (2007) | Nickel Alloy, Corrosion and Heat-Resistant, Wire 72Ni - 15.5Cr - 0.95Cb - 2.5Ti - 0.70Al - 7.0Fe No. 1 Temper, Precipitation Hardenable | SAE-AMS-5698G-(2007).pdf |
SAE AMS 5699G (2007) | Nickel Alloy, Corrosion and Heat-Resistant, Wire 72Ni - 15.5Cr - 0.95Cb - 2.5Ti - 0.70Al - 7.0Fe Spring Temper, Precipitation Hardenable | SAE-AMS-5699G-(2007).pdf |
SAE AMS 5747D (2006) | Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 72Ni - 15.5Cr - 0.95Cb(Nb) - 2.5Ti - 0.70Al - 7.0Fe Solution Heat Treated, Precipitation Hardenable | SAE-AMS-5747D-(2006).pdf |
SAE AMS 5779E (2003) | Alloy Welding Electrodes, Covered, Corrosion and Heat-Resistant 75Ni - 15Cr - 1.5 (Cb+Ta) - 1.9Ti - 0.55Al - 5.5Fe | SAE-AMS-5779E-(2003).pdf |
SAE AMS 5583E (2013) | Nickel Alloy, Corrosion and Heat-Resistant, Seamless Tubing 72Ni - 15.5Cr - 0.95Cb - 2.5Ti - 0.70Al - 7.0Fe Vacuum Melted Solution Heat Treated, Precipitation Hardenable to 170 ksi (1172 MPa) Tensile Strength | SAE-AMS-5583E-(2013).pdf |
SAE J 467b (1968) | Special Purpose Alloys ("Superalloys") | SAE-J-467b-(1968).pdf |
SAE J 470 (1976) | Wrought nickel and nickel-related alloys | SAE-J-470-(1976).pdf |