USA AMS SAE AMS 5589F (2013), SAE AMS 5590F (2010), SAE AMS 5597F (2009), SAE AMS 5664E (2006), SAE AMS 5832G (2010), SAE AMS 5917 (2011), Inconel 718 Superalloys Nickel Alloy, Corrosion and Heat-Resistant, Seamless Tubing 52.5Ni - 19Cr - 3.0Mo - 5.1Cb (Nb) - 0.90Ti - 0.50Al - 18Fe Consumable Electrode Remelted or Vacuum Induction Melted 1775°F (968°C) Solution Heat Treated and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Class | Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Superalloys | Inconel 718 | AMS | USA | Nickel Alloy, Corrosion and Heat-Resistant, Seamless Tubing 52.5Ni - 19Cr - 3.0Mo - 5.1Cb (Nb) - 0.90Ti - 0.50Al - 18Fe Consumable Electrode Remelted or Vacuum Induction Melted 1775°F (968°C) Solution Heat Treated |
C | Cr | Mo | Ni | Al | Nb | Fe | Si | Mn | P | S | B |
---|---|---|---|---|---|---|---|---|---|---|---|
≤0.03 | 17.0 -21.0 | 2.80 -3.30 | 50.0 -55.0 | 0.20 -0.60 | 4.75 -5.50 | ≤Bal | ≤0.35 | ≤0.35 | ≤0.015 | ≤0.015 | ≤0.006 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
815 (≥) | 797 (≥) | 23 | 33 | 33 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 443 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
14 | - | - | 0.31 | - | |||
452 | 697 | - | 14.3 | 224 | - | ||
213 | - | 32 | 34.2 | 242 | 232 |
Heat treated : 1554°C - 1615°C
Grade | Standard | Country | Application |
---|---|---|---|
NiCr19Fe19Nb5Mo3 |
SAE AMS 5589F (2013) | Nickel Alloy, Corrosion and Heat-Resistant, Seamless Tubing 52.5Ni - 19Cr - 3.0Mo - 5.1Cb (Nb) - 0.90Ti - 0.50Al - 18Fe Consumable Electrode Remelted or Vacuum Induction Melted 1775°F (968°C) Solution Heat Treated | SAE-AMS-5589F-(2013).pdf |
SAE AMS 5590F (2010) | Nickel Alloy, Corrosion and Heat Resistant, Seamless Tubing 52.5Ni - 19Cr - 3.0Mo - 5.1Cb - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1950°F (1066°C) Solution Heat Treated | SAE-AMS-5590F-(2010).pdf |
SAE AMS 5597F (2009) | Nickel Alloy, Corrosion and Heat Resistant, Sheet, Strip, and Plate 52.5Ni - 19Cr - 3.0Mo - 5.1Cb - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1950°F (1066°C) Solution Heat Treated | SAE-AMS-5597F-(2009).pdf |
SAE AMS 5664E (2006) | Nickel Alloy, Corrosion and Heat Resistant, Bars, Forgings, and Rings 52.5Ni - 19Cr - 3.0Mo - 5.1Cb - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1950°F (1066°C) Solution Heat Treated, Precipitation Hardenable | SAE-AMS-5664E-(2006).pdf |
SAE AMS 5832G (2010) | Nickel Alloy, Corrosion and Heat Resistant, Welding Wire 52.5Ni - 19Cr - 3.0Mo - 5.1Cb - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted | SAE-AMS-5832G-(2010).pdf |
SAE AMS 5917 (2011) | Metal Injection Molded Nickel Based, Alloy 718 Parts, Hot Isostatically Pressed, Solutioned and Aged | SAE-AMS-5917-(2011).pdf |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com