USA ASTM B 983 (2013), B 983 N07718 Superalloys Precipitation Hardened or Cold Worked, Seamless Nickel Alloy Pipe and Tube and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Class | Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Superalloys | B 983 N07718 | ASTM | USA | Precipitation Hardened or Cold Worked, Seamless Nickel Alloy Pipe and Tube |
C | Cr | Mo | Ni | Al | Nb | Fe | Si | Mn | P | S | B |
---|---|---|---|---|---|---|---|---|---|---|---|
≤0.03 | 17.0 -21.0 | 2.80 -3.30 | 50.0 -55.0 | 0.20 -0.60 | 4.75 -5.50 | ≤Bal | ≤0.35 | ≤0.35 | ≤0.015 | ≤0.015 | ≤0.006 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
199 (≥) | 318 (≥) | 34 | 22 | 21 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 321 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
12 | - | - | 0.43 | - | |||
383 | 864 | - | 31.3 | 124 | - | ||
572 | - | 31 | 33.2 | 142 | 134 |
Heat treated : 1216°C - 1311°C
Grade | Standard | Country | Application |
---|---|---|---|
NiCr19Fe19Nb5Mo3 |
B 983 (2013) | Precipitation Hardened or Cold Worked, Seamless Nickel Alloy Pipe and Tube | B-983-(2013).pdf |