China JB GH 3536 Superalloys Superalloy GH536 is a kind of added tungsten cobalt and nickel - chromium - molybdenum alloy.GH536 alloy at 1200 ℃ with excellent oxidation resistance at high temperature, also can be applied to the neutral and reducing atmosphere.At the same time GH536 a and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Class | Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Superalloys | GH 3536 | JB | China | Superalloy GH536 is a kind of added tungsten cobalt and nickel - chromium - molybdenum alloy.GH536 alloy at 1200 ℃ with excellent oxidation resistance at high temperature, also can be applied to the neutral and reducing atmosphere.At the same time GH536 a |
Ni | Cr | Fe | C | Mn | Si | Mo | Co | Al | W | B | P | S |
---|---|---|---|---|---|---|---|---|---|---|---|---|
≤Bal | 20.50 -23.50 | 17.00 -20.00 | 0.05 -0.15 | ≤1.00 | ≤1.00 | 8.00 -10.00 | 0.50 -2.50 | ≤0.10 | 0.20 -1.00 | ≤0.005 | ≤0.015 | ≤0.01 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
491 (≥) | 397 (≥) | 11 | 24 | 22 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 313 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
41 | - | - | 0.14 | - | |||
271 | 298 | - | 32.3 | 242 | - | ||
375 | - | 14 | 24.2 | 213 | 421 |
Heat treated : 1368°C - 1567°C
Grade | Standard | Country | Application |
---|---|---|---|
N06002 | |||
UNS N06002 | |||
UNS N06002 | |||
UNS N06002 |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com