Chemical composition(mass fraction)(wt.%) of the NITRONIC 60

 

C
Si
Mn
P
S
Cr Ni
0.1 3.5-4.5 7-9     16-18 8-9
Mo Al Cu Nb Ti V Ce
             
N Co Pb B Other    
0.08-0.18            
             

 

Nitronic 60 physical properties:

 

density

8.0 g/cm3

 

Melting point

1375 ℃

 Nitronic 60 at normal temperature alloy of the mechanical properties of the minimum:

 state

Tensile strength Rm N/was

The yield strength RP0.2 N/was

Elongation A5 %

Brinell hardness HB

 

Solid melting state

690

380

35

More than 241

 Nitronic 60 characteristics:

 With cobalt and high nickel alloy, compared to Nitronic 60 stainless steel with very low cost can realize the corrosion resistance and wear resistance. Its overall better than most medium corrosion resistance of 304 type. In Nitronic 60, of the ability of pitting chloride better than 316 type.

 The yield strength at room temperature is almost 304 and 316 two times.
Nitronic 60 have excellent resistance to high temperature oxidation resistance and impact resistance to low temperature.
Nitronic 60 application:

 Widely used in electric power, chemical, petrochemical, food and oil and gas industry, including expansion joint wear-resistant plate, wear-resisting pump ring, bushings, process stem, seal and logging equipment.

Mechanical Properties of steel grade NITRONIC 60

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV/Ku (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
826 (≥) 232 (≥) 12 42 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 211

Physical Properties of steel grade NITRONIC 60

Temperature
(°C)
Modulus of elasticity
(GPa)
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and Thermal conductivity
(W/m·°C)
Specific thermal capacity
(J/kg·°C)
Specific electrical resistivity
(Ω mm²/m)
Density
(kg/dm³)
Poisson’s coefficient, ν
24 - -     0.21 -  
455 616 - 41.3 324   -  
873 - 41 23.2   331 413

Heat Treatment of steel grade NITRONIC 60

Heat treated : 1542°C - 1361°C

Technological Curves of steel grade NITRONIC 60

Cross Reference Table (Equivalent Grade) of NITRONIC 60

Grade Standard Country Application
UNS G10060 UNS USA General use carbon steel bar
UNS G10160 UNS USA General use carbon steel bar
T41901 UNS USA Alloy tool steel
T51602 UNS USA Alloy tool steel
ASP60 AISI USA Powder metallurgy high-speed tool steel
HAP 60 AISI USA Powder metallurgy high-speed tool steel
C-60 AISI USA Machining with carbide
C60W DIN Germany Carbon tool steel
60WCrV7 DIN Germany Cold working alloy tool steel
1.2601 DIN Germany Cold working alloy tool steel
1.2604 DIN Germany Cold working alloy tool steel
60NiCrMoV12-4 DIN Germany Cold working alloy tool steel
60MnSiCr4 DIN Germany Cold working alloy tool steel
1.2360 DIN Germany Hot working alloy tool steel
1.2603 DIN Germany Hot working alloy tool steel
1.2606 DIN Germany Hot working alloy tool steel
X60WCrMoV9-4 DIN Germany Hot working alloy tool steel
SK60 JIS Japan Carbon tool steel
BL1 Carbide for cutting tools
BL1 Carbide for cutting tools

Available Suppliers

Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...

Rfq.: sales@longhaisteel.com
  • Do you supply this NITRONIC 60?
  • List your company on S&G now? Join
  • Non-paying users only
Sidebar RFQs Menu My Account
Top